ʻO ke kuʻi ʻana o ka titanium

1. Nā waiwai metala a me nā palena o ka titanium

He liʻiliʻi ka umekaumaha kikoʻī o ka Titanium (ʻo ka umekaumaha kikoʻī he 4.5), ka ikaika kiʻekiʻe, ke kūpaʻa maikaʻi i ke kiʻekiʻe a me ka haʻahaʻa haʻahaʻa, a me ke kūpaʻa māwae maikaʻi loa a me ka pale ʻana i ka corrosion i loko o ka chlorine pulu. ʻO nā mea mechanical a me ka welding o ka titanium e pili ana i ka maʻemaʻe o nā mea titanium. ʻO ke kiʻekiʻe o ka maʻemaʻe, ʻoi aku ka maikaʻi o ka hana. ʻO ka haʻahaʻa o ka maʻemaʻe, ka emi nui o ka plasticity a me ka paʻakikī, a ʻoi aku ka maikaʻi o ka hana kuʻi. He ikaika loa ka Titanium ma luna o 300°C a maʻalahi hoʻi i ka hydrogen, oxygen a me nā ʻātoma nitrogen i nā wela kiʻekiʻe, e hana ʻino ai ka mea. Hoʻomaka ka Titanium e komo i ka hydrogen ma kahi wela kiʻekiʻe o 300°C, oxygen ma 600°C, a me nitrogen ma 700°C.

Pono nā mīkini hoʻoheheʻe Argon arc e loaʻa i ka ʻāʻī arc kiʻekiʻe, ka attenuation o kēia manawa, ka pale ʻana i ke kinoea hoʻopaneʻe, a me nā uea hoʻoheheʻe pulse e pono ai nā waiwai mechanical e like me ka mea makua.
ʻO ka mea o ka uhi pale he kila poni a i ʻole titanium, a pono ke ʻano no ka pale ʻana i ka weld e pale i ka weld mai ka hoʻololi ʻana i ke kala. Pono e hoʻokomo ʻia kahi uea kuhili ʻole i loko o ka uhi pale e pāʻani ai i kahi hana hoʻopaʻa kinoea.

Loaʻa i nā lako wili Xinfa nā hiʻohiʻona o ke kiʻekiʻe kiʻekiʻe a me ke kumu kūʻai haʻahaʻa. No nā kikoʻī, e kipa:Welding & Oki Manufacturers - China Welding & Cutting Factory & Suppliers (xinfatools.com)

2. ʻenehana hana kuʻihao Titanium

Hoʻomaʻemaʻe ma mua o ka wili ʻana:
Hoʻopili ʻia ka mea me ka mīkini kihi ʻōwili, a ʻo ka unahi oxide, grease, burrs, dust, etc. i loko o 25mm ma nā ʻaoʻao ʻelua e poni ʻia me kahi pulupulu uea, a laila holoi ʻia me ka acetone a i ʻole ethanol.

Palena welding:

Ma mua o ka wili ʻana, pono ʻoe e aʻo mua i ka pale argon. I ka pale ʻana, paʻa kekahi i ka uhi pale e pale i ka ʻaoʻao luna, a paʻa kekahi i ka uhi pale e pale i ka ʻaoʻao lalo. Pono ka mea pale e hui pū me ka welder. Ma hope o ka wili, hiki ke hoʻokuʻu wale ʻia ka uhi pale ma hope o ka maʻalili ʻana o ka weld. No ka wiliwili ʻaoʻao hoʻokahi a me ka hoʻokumu ʻana i nā ʻaoʻao ʻelua, pono e uku ʻia ka nānā kūikawā i ka pale o ka ʻaoʻao hope. Inā ʻaʻole i mālama maikaʻi ʻia, ʻaʻole hiki ke kahe ka wai welding, a ʻaʻohe hana.
I ka wā e kuʻi ai, pono e loaʻa i ka weld ka lawa o 3-5mm e hana i kahi lua arc. E paʻa i ka pū wili ma kou lima ʻākau a e hoʻāʻo e hoʻohaʻahaʻa i ka electrode tungsten o ka pū wili. E hoʻopaʻa i ka uea kuʻi ma kou lima hema a hoʻohana i kou manamana nui a me kou manamana lima waena e hoʻopaʻa i ka uwea wili a hoʻouna i mua. I ka hoʻouna ʻana i ka uwea welding, pono ʻoe e mālama i ka hoʻomau a me ke kūpaʻa. Pono nā lima ʻelua e hoʻopaʻa paʻa i ka weld. E nānā mau nā maka i ka hohonu o ka wai hoʻoheheʻe a me ke kahe ʻana o ka wai wili. Pono e hoʻoponopono ʻia ke au e like me nā lula a pāpā ʻia ka nui o ke au.

Mālama ʻia ke kinoea argon nozzle ma 5ml, mālama ʻia ke kinoea pale ma 25ml, a mālama ʻia ke kua ma 20ml e hōʻoia i ka hoʻololi ʻole o ka weld i ke kala ma hope o ka uhi pale. Ke kuʻi ʻelua ʻelua, pono e waiho ʻia kahi manawa hoʻomaha e hoʻemi i ka mahana o ka ʻili ma lalo o 200 ℃, inā ʻaʻole hiki ke maʻalahi nā māwae a me ka brittleness. Pono e hoʻohana ʻia ka wiliwili pālahalaha a me ka nozzle rotation welding e like me ka hiki.

I ka wā e wili ai, pono e maloʻo ka lumi a me ka lepo ʻole, ʻo ka wikiwiki o ka makani e emi iho ma mua o 2 mika / kekona, a hiki i nā makani ikaika ke hana maʻalahi i ka arc instability. I ka hoʻopaʻa ʻana i ka weld, e hoʻāʻo e hoʻohana i kahi mea pulse e hoʻonani ai i ka weld.

a

3. Ke kaʻina hana a me ka ʻenehana mālama ʻana i nā mea hana titanium

ʻO nā mea i hoʻohana ʻia no ka hana ʻana i nā paipu titanium, nā kuʻekuʻe titanium, a me nā pahu titanium pono e hoʻokō i nā koi. ʻO ko lākou paʻakikī, ikaika, a me ka elasticity pono e loaʻa kahi palapala palapala. Pono e hoʻoponopono ʻia kēlā me kēia pā titanium me kahi lula. Pono e helu ʻia ka nui i ka wā e ʻoki ai i nā mea i mea e pale ai i nā ʻōpala keu. Pono e hoʻohana ʻia nā mīkini ʻāhi i ka wā e ʻoki ai i nā pā, a e pale ʻia ka ʻoki kinoea e like me ka hiki. Pono e hōʻailona pono ʻia nā laina i ka wā e hoʻohana ai i nā pipeline. Ua pāpā loa ʻia ka hoʻohana pinepine ʻana i ka ʻoki kinoea. Ma hope o ka ʻoki ʻana i ka pā, pono e hoʻohana ʻia ka mīkini chamfering e hana i ke awāwa. Pono nā māwae. Ma hope o ka ʻōwili ʻia ʻana o ka pā e ka mīkini ʻōwili pā no ka manawa mua, pono e hoʻokaʻawale iki ka weld e hoʻomaʻamaʻa i ka lua o ka hoʻopulapula ʻana. No ka mea he kiʻekiʻe ke kumukūʻai o nā mea titanium (e pili ana i 140 yuan / Kg no nā mea maka a ma kahi o 400 yuan / Kg ma hope o ka hana ʻana), pono e pale ʻia ka ʻōpala.

Aia kahi ʻokoʻa nui ma waena o ka mālama ʻana a me ka hoʻoili ʻana o nā papa titanium. ʻO nā kumu nui e pili ana i nā mea kūlohelohe, nā hoʻololi waiwai, a me nā mea ʻē aʻe. Pono e pale ʻia ka weld inā hiki ke pale ʻia. Inā ʻaʻole hiki ke pale i nā ʻaoʻao ʻelua, e hoʻohana i ka pale liʻiliʻi i kēia manawa hoʻokahi ʻaoʻao. Ma hope o nā māwae weld, mai weld i ka weld kumu. Pono e hana ʻia ke kuʻi ʻana ma ka paʻi ʻana i ka pā. I ka makani ʻana o ke kahua hoʻoheheʻe ʻia, pono e loaʻa kahi malu makani, a ʻo ka tarpaulin a i ʻole ka pā hao no ka pale. I ka lawe ʻana i ka paipu, pono e loaʻa kahi āpau a i ʻole ka hoʻoheheʻe ʻana no ka mea ʻaʻole hiki ke pale ʻia ka loko. Pono e hoʻonui a mānoanoa ka weld.